2K EP Primer Gray (-B- Component) - 1000kg IBC

Login to view prices
Delivery time: 1-3 Business Days
  • Suitable for almost all rigid substrates and applications such industrial floors, commercial and production facilities, warehouses, sterile floor areas, etc.
  • Applied as a roller primer
  • Compatible with EP Levelling Compound, EP Industry, EP Design, PU Flex, and PU Design
  • Floor texture remains visible after coating
  • Consumption: approx. 330 g/m²
  • Walkable / recoatable after approx. 14 hours, fully load-bearing after approx. 7 days (at +20 °C)

Instructions for Use

chevronBottom

Prepare substrate:

The substrate must be level, load-bearing, dry, sufficiently tensile and compressive strength, and clean. Dust, oil, grease and release agents must be removed in advance using suitable methods (preferred method: shot blasting; alternatively diamond grinding with thorough vacuuming).
Application should be carried out at 10-30 °C (room and substrate temperature) and a maximum relative humidity of 70 %.

Apply EP Primer:

  1. For mixing, pour the complete contents of EP Primer component B into the container of EP Primer component A and mix slowly and thoroughly with a drill for approx. 3 minutes at 300-400 rpm.
    Working Time: approx. 40 minutes at 20 °C.
  2. Immediately after mixing, pour the material onto the floor, spread it with a rubber squeegee and then roll over it to achieve an even surface and retain the floor texture.
  3. During curing, protect the area from moisture, dust and mechanical stress. Walkable after approx. 14 hours, fully load-bearing after approx. 7 days (temperature-dependent).

Apply EP Levelling Compound, EP Industry, EP Design, PU Flex or PU Design:

Subsequent coating with other products may be applied at 20 °C no earlier than 14 hours and no later than 36 hours after application of the EP Primer.
Important: If the subsequent coating is not applied within 36 hours, the EP Primer must be broadcast with quartz sand while still fresh/liquid (recommended amount: approx. 300 g/m²).
Before applying the next coating, any loose excess quartz sand must be removed with a broom.

Important Notes

chevronBottom

Colour deviations are possible due to raw material variations. When using different batches, base components should be pre-mixed. UV radiation and weathering may cause slight colour changes. To avoid curing and mixing problems, components A and B must first be thoroughly mixed, then transferred into a second clean container and mixed again.

Danger

chevronBottom

Causes skin irritation. Causes serious eye irritation. May cause an allergic skin reaction. May damage fertility. Toxic to aquatic life with long lasting effects. Harmful if swallowed. Causes severe skin burns and eye damage. May cause damage to organs ( state all organs affected, if known) through prolonged or repeated exposure (state route of exposure if it is conclusively proven that no other routes of exposure cause the hazard). Harmful to aquatic life with long lasting effects. Contains epoxy constituents. May produce an allergic reaction. The information on the product label must always be followed.

piktogram-ausrufezeichen-fisch-reagenzglas-giftlunge.png